No Profanity *** No Flaming *** No Advertising *** No Anti Trappers ***NO POLITICS
No Non-Target Catches *** No Links to Anti-trapping Sites *** No Avoiding Profanity Filter


Home~Trap Talk~ADC Forum~Trap Shed~Wilderness Trapping~International Trappers~Fur Handling

Auction Forum~Trapper Tips~Links~Gallery~Basic Sets~Convention Calendar~Chat~ Trap Collecting Forum

Trapper's Humor~Strictly Trapping~Fur Buyers Directory~Mugshots~Fur Sale Directory~Wildcrafting~The Pen and Quill

Trapper's Tales~Words From The Past~Legends~Archives~Kids Forum~Lure Formulators Forum~ Fermenter's Forum


~~~ Dobbins' Products Catalog ~~~


Minnesota Trapline Products
Please support our sponsor for the Trappers Talk Page - Minnesota Trapline Products


Print Thread
Hop To
Page 2 of 2 1 2
Re: battery acid tanning question [Re: foxkidd44] #7016765
10/13/20 09:02 PM
10/13/20 09:02 PM
Joined: Aug 2010
Posts: 4,483
PA
P
PAskinner Offline
trapper
PAskinner  Offline
trapper
P

Joined: Aug 2010
Posts: 4,483
PA
Rittels safety acid works great and isn't dangerous like battery acid.


Right now I’m having amnesia and déjà vu at the same time. I think I’ve forgotten this before.
Re: battery acid tanning question [Re: Boco] #7016768
10/13/20 09:03 PM
10/13/20 09:03 PM
Joined: Jan 2008
Posts: 9,154
Alaska and Washington State
W
waggler Offline
trapper
waggler  Offline
trapper
W

Joined: Jan 2008
Posts: 9,154
Alaska and Washington State
Originally Posted by Boco
90% of leather today is chrome tanned.

Chrome tan is good for leather but most people don't use it for fur products since it turns the leather bluish-green. It can be dyed thought, usually some shade of brown.


"My life is better than your vacation"
Re: battery acid tanning question [Re: foxkidd44] #7017020
10/14/20 07:10 AM
10/14/20 07:10 AM
Joined: Jun 2007
Posts: 4,674
Illinois
foxkidd44 Offline OP
trapper
foxkidd44  Offline OP
trapper

Joined: Jun 2007
Posts: 4,674
Illinois
I was able to find a correct recipie that would give me a ph of around 1.5 using battery acid. from what I was told. "use 1/2 pound or 8 ounces of salt and 1/2 ounce by weight of battery acid or sulfuric acid you will end up with a pH of 1.2 and this is very desirable for properly charging the Hide for tanning and cleaning out the unwanted‘s ".


Stand by your principles, Stand by your guns, and victory complete and permanent is sure at last.